Research Article
Mechanical Damage Test and Model Study of Layered Composite Rock Based on Acoustic Emission and DIC Characteristics
Table 4
Parameters and numbers of specimens.
| Specimens | Length (mm) | Radius (mm) | Quality (g) | Density (g·cm−3) | Test type |
| S-1-AB | 99.82 | 49.15 | 393.38 | 2.08 | Applied acoustic emission system monitoring | S-2-AB | 99.15 | 49.26 | 391.45 | 2.07 | S-3-AB | 99.20 | 49.31 | 392.84 | 2.07 | S-4-AB | 98.54 | 49.58 | 393.12 | 2.07 | S-5-A | 99.21 | 49.16 | 402.16 | 2.14 | S-6-A | 100.12 | 49.25 | 410.72 | 2.15 | S-7-B | 101.06 | 49.17 | 390.38 | 2.04 | S-8-B | 101.14 | 49.15 | 390.16 | 2.03 | 5A-1 | 99.15 | 49.12 | 402.54 | 2.14 | Application of DIC system monitoring, including composite rock combined with acoustic emission monitoring | 5A-2 | 101.11 | 49.15 | 413.37 | 2.16 | 5A-3 | 100.56 | 49.16 | 412.02 | 2.15 | 5AB-1 | 99.28 | 49.22 | 391.66 | 2.07 | 5AB-2 | 99.15 | 49.13 | 389.72 | 2.07 | 5AB-3 | 99.24 | 49.11 | 390.47 | 2.08 | 5B-1 | 98.45 | 49.12 | 378.63 | 2.03 | 5B-2 | 99.98 | 48.96 | 379.72 | 2.02 | 5B-3 | 99.65 | 49.24 | 387.56 | 2.04 |
|
|