Research Article

Synthesis and Photocatalytic Properties of ZnWO4 Nanocrystals via a Fast Microwave-Assisted Method

Figure 6

Typical nitrogen adsorption isotherms of as-prepared ZnWO4: (a) 140°C and (b) 160°C. Inset: Effect picture of photocatalytic degradation RhB by ZnWO4 prepared at 140°C for 5 min.
458106.fig.006