Research Article

Evaluation of Fatigue Life of CRM-Reinforced SMA and Its Relationship to Dynamic Stiffness

Table 3

SMA 20 aggregate gradation [4].

BS sieveMin.%Passing%RetainedWeight (G)
Max.Mid.

1910010010000
12.585959010110
9.565757020220
4.7520282446506
2.36162420444
0.6121614666
0.3121513.50.55.5
0.07581094.549.5
Pan000999
1001100