Research Article
Evaluation of Fatigue Life of CRM-Reinforced SMA and Its Relationship to Dynamic Stiffness
Table 4
Properties of coarse and fine aggregate.
| Properties | Standard test | Test results | Standard requirement |
| L.A. abrasion () | ASTM C-131 | 21% | Below 30% | Flakiness index () | BS 182: part 3 | 4% | Below 20% | Elongation index () | BS 182: part 3 | 14.3% | Below 20% | Soundness () | BS 12: part 3 | 4.1% | Below 12% | Impact value () | BS 12: part 3 | 12.4% | Below 15% | Polished stone value () | BS 12: part 3 | 48.4% | Above 40% |
|
|