Research Article

Wear Behavior of Aluminium Metal Matrix Composite Prepared from Industrial Waste

Figure 12

(a) SEM of worn surface of sample-III after running 3000 m at 29.43 N load and 4.71 m/s sliding speed. (b) XRD test report of the worn surface of sample-III.