Research Article
Wear Behavior of Aluminium Metal Matrix Composite Prepared from Industrial Waste
Figure 13
(a) SEM of sample-II at higher magnification before wear test. (b) SEM of wear track of sample-II at higher magnification after wear test (after running 2000 m at 29.43 N load and 4.71 m/s sliding speed).
(a) |