Research Article
H2S Loss through Nalophan™ Bags: Contributions of Adsorption and Diffusion
Table 2
Experimental conditions. The bag tested was without any film inside (B-no film) and with the film inside. The surface of the internal film sheet was equal to 1900 cm2 (B-film 1900), 2580 cm2 (B-film 2580), and 3520 cm2 (B-film 3520) respectively.
|