The experimental parameters and weight loss of 316L steel exposed to two different environments.
| Test condition | Without H2S | With H2S |
| Temperature (°C) | 60 | Partial pressure H2S (bar) | 0 | 3 | Total pressure (bar) | 30 |
| pH (before/after) | 2.52/2.63 | 2.95/3.42 | Weight loss (g) | 0.01 | 0.086 | Immersion time | 7 days (128 h) | Solution | NACE TM0177 solution A (5wt% NaCl and 0.5wt% CH3COOH in distilled water) |
|
|