Research Article

Water Absorption, Thermal, and Mechanical Properties of Bamboo Fiber with Chopped Glass Fiber Filler-Reinforced Polyester Composites

Figure 11

Strain-stress curve of flexural strength at (a) 30 wt.% (b) 35 wt.% (c) 40 wt.% bamboo fiber content of BPRPEC with chopped glass fiber filler.
(a)
(b)
(c)