Research Article
Water Absorption, Thermal, and Mechanical Properties of Bamboo Fiber with Chopped Glass Fiber Filler-Reinforced Polyester Composites
Table 24
ANOVA and significance of each parameter on impact strength for BPRPEC with CGF filler.
| Source | Sum of squares | Df | Mean-square | F-value | -value | Significance |
| Quadratic model | 3883.56 | 5 | 776.71 | 153.73 | 0.0008 | Significant | A-BF wt.% | 3471.38 | 1 | 3471.38 | 687.06 | 0.0001 | Significant | B-CGF wt.% | 163.07 | 1 | 163.07 | 32.28 | 0.0108 | Significant | AB | 29.81 | 1 | 29.81 | 5.90 | 0.0073 | Insignificant | | 215.49 | 1 | 215.49 | 42.95 | 0.4491 | Insignificant | | 3.81 | 1 | 3.81 | 0.7538 | | | Residual | 15.16 | 3 | 5.05 | | | | Cor total | 3898.72 | 8 | | | | |
|
|