Research Article

Optimizing the Dry Sliding Wear Behavior of Stir-Casted Al6061/Nano-Al2O3/Quartz Hybrid Metal Matrix Composite Using Taguchi Method

Table 7

Analysis of variance for wear rate (mm3/m).

SourceDFSeq SSAdj SSAdj MSFPPr

Applied load (N)2187.536187.53693.76781803.790.00287.83%
Rotational speed (rpm)221.49421.49410.7469206.740.001910.06%
Weight percentage of reinforcement23.4333.4331.716333.020.6461.60%
Error201.0401.0400.0520