Corrosion Behaviour of a Cr2O3 Coating on Mild Steel in Synthetic Mine Water
Table 3
EDX analyses (in wt%) of Cr2O3 coating and mild steel substrate surfaces taken from Figure 6 after potentiodynamic polarisation in synthetic mine water at pH 6, 3, and 1 [26].