Research Article
Post-Fracture Stiffness and Residual Capacity Assessment of Film-Retrofitted Monolithic Glass Elements by Frequency Change
Figure 2
Schematic setup and operational steps for the current experimental investigation (with L = 100 mm, Lb = 95 mm, t = 6 mm, and Lc,1 ≈ 0.5 Lb).