Research Article
Titanium Oxide: A Bioactive Factor in Osteoblast Differentiation
Figure 1
SEM images of Ti-6Al-4V and γ-TiAl alloys. (a), (b): untreated, (c), (d): oxidized at 500°C, (e), (f): oxidized at 800°C, and (g), (h): MAO at 225 mA, 4 mins.
| (a) |
| (b) |
| (c) |
| (d) |
| (e) |
| (f) |
| (g) |
| (h) |