Research Article
Titanium Oxide: A Bioactive Factor in Osteoblast Differentiation
Table 1
Average roughness values (in
m) measured on Ti alloy sample surfaces for various treatments using AFM.
| | Treatment | Ti-6Al-4V | -TiAl |
| | None | 51.74 | 49.30 | | Oxidation at 500°C | 102.40 | 31.34 | | Oxidation at 800°C | 318.80 | 65.88 | | MAO 200 mA, 3 min | 246.30 | 174.50 | | MAO 200 mA, 4 min | 247.60 | 185.90 | | MAO 225 mA, 3 min | 213.30 | 137.50 | | MAO 225 mA, 4 min | 301.70 | 189.80 |
|
|