Research Article
Influence of Various Chemical Surface Treatments, Repair Materials, and Techniques on Transverse Strength of Thermoplastic Nylon Denture Base
Table 2
Mean and standard deviation (SD) of transverse strength of nylon base repaired with different materials, curing techniques, and surface treatments.
| | Repair technique | Surface treatments | N | Mean (N/mm2) | SD |
| | Microwave heat-polymerized | Monomer | 10 | 18.29 | 6.62 | | Isopropyl | 10 | 13.48 | 1.43 | | Acetone | 10 | 10.39 | 2.19 | | Ethyl acetate | 10 | 10.92 | 1.83 | | Control (without surface treatment) | 10 | 8.47 | 0.86 |
| | Ivomate autopolymerized | Monomer | 10 | 10.39 | 1.13 | | Isopropyl | 10 | 10.18 | 2.35 | | Acetone | 10 | 7.37 | 1.47 | | Ethyl acetate | 10 | 8.07 | 1.11 | | Control (without surface treatment) | 10 | 7.09 | 1.82 |
| | Light curing | Monomer | 10 | 9.44 | 2.21 | | Isopropyl | 10 | 6.37 | 0.90 | | Acetone | 10 | 6.26 | 1.02 | | Ethyl acetate | 10 | 6.13 | 1.14 | | Control (without surface treatment) | 10 | 5.58 | 1.61 |
|
|