Research Article
Effect of Different Surface Treatments on the Micro-Shear Bond Strength and Surface Characteristics of Zirconia: An In Vitro Study
Table 7
Post hoc Tukey test for the translucent groups showing significant difference.
| Dependent variable | Comparison group | Compared with | Mean difference | Standard error | Value |
| Micro-shear bond strength (µSBS) | TC | TA | −2.536 | 2.13658 | 0.639 | TE | −5.3 | 2.13658 | 0.08 | TAE | −9.17800 | 2.13658 | 0.001 | TA | TE | −2.764 | 2.13658 | 0.573 | TAE | −6.64200 | 2.13658 | 0.018 | TE | TAE | −3.878 | 2.13658 | 0.283 |
|
|