Research Article

An In Vitro Study on the Shear Bond Strength of Feldspathic Porcelain to Nickel Chromium Alloy and Cobalt Chromium Alloy after Various Surface Treatments

Table 2

Post hoc comparison between groups based on shear bond strength of Ni-Cr alloy samples using post hoc Tukey’s tests.

GroupMean differenceStandard error95% confidence interval
value
Lower boundUpper bound

Group 1Group 2−5.180.54719−6.65−3.70.001
Group 1Group 3−18.42−19.89−16.950.001
Group 1Group 4−9.39−10.86−7.910.001
Group 2Group 3−13.24−14.71−11.770.001
Group 2Group 4−4.21−5.68−2.730.001
Group 3Group 49.037.5510.50.001

, significant; , highly significant; , very highly significant; , not significant.