Research Article

An In Vitro Study on the Shear Bond Strength of Feldspathic Porcelain to Nickel Chromium Alloy and Cobalt Chromium Alloy after Various Surface Treatments

Table 4

Post hoc comparison between groups based on shear bond strength of Co-Cr alloy samples using post hoc Tukey’s tests.

GroupMean differenceStandard error95% confidence interval value
Lower boundUpper bound

Group 1Group 2−6.390.62279−8.07−4.710.001
Group 1Group 3−19.21−20.89−17.540.001
Group 1Group 4−10.39−12.06−8.710.001
Group 2Group 3−12.82−14.5−11.140.001
Group 2Group 4−3.99−5.67−2.310.001
Group 3Group 48.827.1510.50.001

, significant; , highly significant; , very highly significant; , not significant.