Antimicrobial and Mechanical Properties of Orthodontic Acrylic Resin Containing Zinc Oxide and Titanium Dioxide Nanoparticles Supported on 4A Zeolite
Table 3
Descriptive values of flexural strength (MPa).
| Group | N | Mean | Std. deviation | Std. error | 95% confidence interval for mean | Lower bound | Upper bound |
| TiO2/ZnO/4A 2% (G1) | 5 | 60.0140 | 3.07822 | 1.37662 | 56.1919 | 63.8361 | ZnO/4A 2% (G2) | 5 | 62.6440 | 4.41532 | 1.97459 | 57.1617 | 68.1263 | TiO2/4A 2% (G3) | 5 | 56.1320 | 2.90165 | 1.29766 | 52.5291 | 59.7349 | TiO2/ZnO/4A 4% (G4) | 5 | 71.9000 | 1.83154 | .81909 | 69.6258 | 74.1742 | TiO2/4A 4% (G5) | 5 | 61.2380 | 3.77233 | 1.68704 | 56.5540 | 65.9220 | ZnO/4A 4% (G6) | 5 | 65.7460 | 7.44352 | 3.32884 | 56.5037 | 74.9883 | Control (G7) | 5 | 85.8560 | 4.58846 | 2.05202 | 80.1587 | 91.5533 | Total | 35 | 66.2186 | 10.15395 | 1.71633 | 62.7306 | 69.7066 |
|
|