Research Article
Influence of Acidic Environmental Conditions on Push-Out Bonding Strength of Four Calcium Silicate-Based Materials to Root Dentin
Figure 7
Mean dislocation resistance (MPa) of repair materials after storage in designated subgroups. ERRM, MTA, and Biodentine show the highest MPa values in 34 days of storage in PBS (group C), whereas bioMTA shows the highest values in 4 days of storage in PBS (group A).