Fracture Resistance of Endodontically Treated Maxillary Premolar Teeth Restored with Wallpapering Technique: A Comparative In Vitro Study

Table 2

One-way ANOVA test for comparison of fracture resistance among the different groups.

ANOVASum of squaresdfMean squareFSig.

Between groups11,218,135.40042,804,533.85076.9060.000
Within groups1,276,346.5003536,467.043
Total1,2494,481.90039