Effect of Finishing Protocols on the Surface Roughness and Fatigue Strength of a High-Translucent Zirconia

Table 1

Mean fatigue strength (MPa) and cycles to fracture of the studied groups.

GroupsMean fatigue strength (MPa)CI

C172.50C159.43–185.56
C + G192.75B186.61–198.88
G243.00A222.36–263.63

Note: Different letters indicate statistically significant differences in the column. Means and 95% confidence intervals (CI).