Research Article
Effect of Finishing Protocols on the Surface Roughness and Fatigue Strength of a High-Translucent Zirconia
Table 2
Survival probability (%) of experimental groups according to applied load and number of cycles.
| Fracture load (N)/cycles | C | C + G | G |
| 120/20,000 | 0.95 | 1 | 1 | 135/40,000 | 0.85 | 1 | 1 | 150/60,000 | 0.60 | 1 | 1 | 165/80,000 | 0.50 | 0.95 | 0.95 | 180/100,000 | 0.35 | 0.65 | 0.95 | 195/120,000 | 0.20 | 0.20 | 0.85 | 210/140,000 | 0.05 | 0.05 | 0.75 | 225/160,000 | 0 | 0 | 0.50 | 240/180,000 | — | — | 0.35 | 255/200,000 | — | | 0.25 | 270/220,000 | — | — | 0.15 | 285/240,000 | — | — | 0.10 | 300/280,000 | — | — | 0.10 | 315/300,000 | — | — | 0.10 | 330/320,000 | — | — | 0.10 | 345/340,000 | — | — | 0.05 | 360/360,000 | — | — | 0.00 |
|
|
Note: Data show the survival probability, where 1 = 100% and 0 = 0%.
|