Studying and Characterization of Coating of Zein–CaSiO3 Composite on Polyetheretherketone Implant Material

Table 8

LSD analysis of adhesion test for all studying groups.

GroupGroupsMean differenceStd. errorSig.

Group 1Group 2−0.200000.227710.388
Group 30.900000.227710.001

Group 2Group 31.100000.227710.000

The mean difference is significant at the 0.05 level.