Research Article

Mechanical Strength, Solubility, and Functional Studies of Developed Composite Biopolymeric Film

Table 3

Selection of WPI concentration as a second base ingredient.

WPI variation (% )Thickness (mm)Moisture content (%)Solubility (%)OpacityColorTensile strength (kgf/cm)Elongation at break (%)
5°C25°C50°C value

0.25daaaadada
0.50cbbbbcbcb
1.0bdcccbcbd
2.0acdddadac

Results are expressed as mean deviation of three determinations. Means in column with different superscript letters differ significantly ().